Micro Palace
![Micro Palace](/image/jp/science/technical/tech/microscopes/electron-microscope/nanoart/1993_2.jpg)
Crystal structure of silicon makes you imagine a micro-palace floating in a sea of clouds.
Prize winning photo at 49th photo contest hosted by the Japanese Society of Electron Microscopy in 1993.
Condition
Specimen: A silicon crystal grain
Instrument: Transmission Electron Microscope H-9000UHR
Magnification : × 800,000
Accelerating voltage : 300 kV
*All information related to these photographers is based on the information when the photo was taken.
*This work was presented at the "photo contest" hosted by the Japanese Society
of Microscopy.
*Reproduction or republication without permission prohibited.
*"nanoart" is registered trademark of Hitachi High-Tech Corporation in Japan.