Micro Bouquet
![Micro Bouquet](/image/jp/science/technical/tech/microscopes/electron-microscope/nanoart/2009_2.jpg)
© Masako Nishimura, atsushi Muto, Yukari Dan, Mari Sakaue (Hitachi High-Tech Corporation)
The small bouquet was found in the electron microscope. This is a SEM image of synthesized zeolite used for a catalyst in a variety of industrial applications. The structure of petal increases surface area and improves performance of catalyzer.
At 65th photo contest hosted by the Japanese Society of Microscopy in 2009.
Condition
Specimen: Synthesized zeolite
Instrument: Ultra-high Resolution Scanning Electron Microscope SU8000
Accelerating voltage: 2kV
*All information related to these photographers is based on the information when the photo was taken.