Dancing peacock
![Dancing peacock](/image/jp/science/technical/tech/microscopes/electron-microscope/nanoart/1999_3.jpg)
This picture was recorded with an SEM using a printed circuit board irradiated by a laser beam. The laser beam is so powerful that it changes structures of many materials. What you can see here may remind you of a peacock with its wings fully opened for welcoming the coming of the 21st century.
At 55th photo contest hosted by the Japanese Society of Electron Microscopy in 1999.
Condition
Specimen : Printed circuit board
Instrument : Cold Field Emission Scanning Electron Microscope S-4700
Magnification : × 2,000
*All information related to these photographers is based on the information when the photo was taken.
*This work was presented at the "photo contest" hosted by the Japanese Society
of Microscopy.
*Reproduction or republication without permission prohibited.
*"nanoart" is registered trademark of Hitachi High-Tech Corporation in Japan.