Warring States Period Picture Scroll
![Warring States Period Picture Scroll - Dark field image of gold leaf of hollow corn beam -](/image/jp/science/technical/tech/microscopes/electron-microscope/nanoart/1996_3.jpg)
© Takuji Miyamoto (Instrument Division, Hitachi, Ltd.)
A dark field image of the gold leaf of hollow corn beam is observed using four diffraction spots of Au {111}. There is atmosphere of battle place in the age of civil wars.
At 52nd photo contest hosted by the Japanese Society of Electron Microscopy in 1996.
Condition
Specimen : Gold leaf
Instrument : Transmission Electron Microscope H-9000NA
Magnification : × 20,000
Accelerating voltage : 300 kV
*All information related to these photographers is based on the information when the photo was taken.
*This work was presented at the "photo contest" hosted by the Japanese Society of Microscopy.
*Reproduction or republication without permission prohibited.
*"nanoart" is registered trademark of Hitachi High-Tech Corporation in Japan.