The escape to the glory
![The escape to the glory](/image/jp/science/technical/tech/microscopes/electron-microscope/nanoart/2003_5.jpg)
This cave is an opening for laser beam of SNOM (Scanning Near-field Optical Microscope) processed in FIB (Focused Ion Beam system) in central part of cantilever in fact, it used for the AFM (Atomic Force Microscope). This SNOM is notified in advanced technologies such as nanotechnology as useful analysis tool.
At 59th photo contest hosted by the Japanese Society of Microscopy in 2003.
Condition
Specimen: An opening for laser beam of SNOM
Instrument: Cold Field Emission Scanning Electron Microscope S-4300
Magnification: × 50,000
Accelerating voltage: 5 kV
Specimen: Courtesy of Nakao Lab., The University of Tokyo.
*All information related to these photographers is based on the information when the photo was taken.
*This work was presented at the "photo contest" hosted by the Japanese Society of Microscopy.
*Reproduction or republication without permission prohibited.