Kyo-komon
![Kyo-komon](/image/jp/science/technical/tech/microscopes/electron-microscope/nanoart/2008_1.jpg)
Pseudo-colored TEM images of H-Nb2O5 thin-film. The pictures were trimmed in A Traditional Japanese Kimono pattern, Kyo-komon. (White dots are vacancy of Nb atomic column.)
Best Photo Prize. At 64th photo contest hosted by the Japanese Society of Microscopy in 2008.
Condition
Specimen: H-Nb2O5
Instrument: Transmission Electron Microscope H-9500
Magnification : ×400,000
Accelerating voltage: 300 kV
*All information related to these photographers is based on the information when the photo was taken.
*This work was presented at the "photo contest" hosted by the Japanese Society
of Microscopy.
*Reproduction or republication without permission prohibited.